Offers high corrosion resistance and the approximate strength of 6061-T6 aluminum. Its high strength to weight ratio give it a diversified field of applications ranging from medical applications to aerospace and automotive fabrication. Typically used in airframe components, cryogenic vessels, heat exchangers, condenser tubing, and pickling baskets.
UNS R50400, commercially pure titanium, CP titanium, C.P. titanium, CP2
Safety Data Sheet | Weight Calculator | Mill Test Reports
Grade 2 Round Bar | Grade 2 Sheet/Plate | Grade 2 Round Tube
ASTM | ASME |
---|---|
B265 | SB265 |
B348 | SB348 |
B338 | SB338 |
Physical Properties Grade 2 | |||||
Density | 0.163 lb/in3 | ||||
Ultimate Tensile Strength | 62.4 ksi | ||||
Yield Tensile Strength | 49.3 ksi | ||||
Shear Modulus | 5,510 ksi | ||||
Shear Strength | 55.1 ksi | ||||
Fatigue Strength | 40.6 ksi | ||||
Hardness Rockwell | Brinell | B89 | 180 | ||||
Elongation at Break Percentage | 26% | ||||
Reduction of Area | 34% | ||||
Modulus of Elasticity | 14,800 ksi | ||||
Poisson's Ratio | 0.34 | ||||
Machinability Percentage | 75% | ||||
Melting Point | 2,930-3,020 °F | ||||
Specific Heat | 1.3 x 10^-1 BTU/lb-°F | ||||
Thermal Conductivity | 156 BTU-in/hr-ft^2-°F | ||||
Electrical Conductivity | 3.6% IACS |
Chemistry Information
|
|
Element |
Percentage |
C | 0.1 max |
Fe | 0.3 max |
H | 0.015 max |
N | 0.03 max |
O | 0.25 max |
Ti | 99.3 min |