An oil or air hardened tool steel that exhibits excellent high impact toughness and strength. Typically used in shear blades, dies, chisels, and punches.
UNS T41907, AISI Type S7, Shock-Resisting Steel, Super-7
Weight Calculator | Mill Test Reports
S7 Drill Rod | S7 Rectangle Bar
ASTM | SAE |
---|---|
A681 | J437 |
S-7 Tool Steel Heat Treatment | ||||
Hardness | Heat Treat Temp. | Quench Medium | Applications | Advantages |
---|---|---|---|---|
As Shipped: Rockwell 90-97B
After Heat Treating: Rockwell 55-57C | 1725°-1750°F | Air or Oil | S7 is good for general tooling and molding applications. It possesses high toughness and shock resistance. | While S7 is very tough compared to other tool steels, it doesn't have hardness comparable to the other tool steels. |
Physical Properties S7 | |||||
Annealed | Hardened | ||||
---|---|---|---|---|---|
Density | 0.283 lb/in3 | 0.283 lb/in3 | |||
Ultimate Tensile Strength | 97 ksi | 290 ksi | |||
Yield Tensile Strength | 53 ksi | N/A | |||
Shear Modulus | 11,000 ksi | 11,000 ksi | |||
Shear Strength | 61 ksi | N/A | |||
Hardness Rockwell | Brinell | B90-97 | 188-223 | C55-57 | 560-595 | |||
Elongation at Break Percentage | 21% | N/A | |||
Modulus of Elasticity | 28,000 ksi | 28,000 ksi | |||
Poisson's Ratio | 0.29 | 0.29 | |||
Machinability Percentage | 95% | N/A | |||
Melting Point | 2,590-2,660 °F | 2,590-2,660 °F | |||
Specific Heat | 1.1 x 10^-1 BTU/lb-°F | 1.1 x 10^-1 BTU/lb-°F | |||
Thermal Conductivity | 276 BTU-in/hr-ft^2-°F | 276 BTU-in/hr-ft^2-°F | |||
Electrical Conductivity | 7.8% IACS | 7.8% IACS |
Chemistry Information
|
|
Element |
Percentage |
Fe | 93.85 |
C | 0.5 |
Cr | 3.25 |
Mo | 1.4 |
Mn | 0.75 |
Si | 0.25 |