Applications | Mechanical and Chemical Data | Tolerances
5083 aluminum is frequently found in marine applications, and is stronger than aluminum 5052 but weaker than 5086. 5083 has superior corrosion resistance, moderate strength, and good formability. 5083 is non-magnetic, easily weldable, and heat treatable. It is typically used in pressure vessels, cryogenics, towers and rigs, oil/gas piping, and armor.
UNS A95083, ISO AlMg4.5Mn, AA5083-H111, Al5083-H111, AA5083-H116, Al5083-H116, AA5083-H131, Al5083-H131
Safety Data Sheet | Weight Calculator | Mill Test Reports
Purchase Round Bar 5083 | Sheet/Plate 5083
Physical Properties 5083 | ||||
-H111 | -H116 | |||
---|---|---|---|---|
Density | 0.096 lb/in3 | 0.096 lb/in3 | ||
Ultimate Tensile Strength | 44 ksi | 47 ksi | ||
Yield Tensile Strength | 21 ksi | 33 ksi | ||
Fatigue Strength | 17 ksi | 23 ksi | ||
Shear Strength | 27 ksi | 28 ksi | ||
Shear Modulus | 3,700 ksi | 3,700 ksi | ||
Hardness Rockwell | Brinell | B41 | 75 | B50 | 83 | ||
Elongation at Break Percentage | 13% | 12% | ||
Modulus of Elasticity | 9,900 ksi | 9,900 ksi | ||
Poisson's Ratio | 0.33 | 0.33 | ||
Machinability Percentage | 30% | 30% | ||
Melting Point | 1,080-1,180 °F | 1,080-1,180 °F | ||
Specific Heat | 2.2 x 10^-1 BTU/lb-°F | 2.2 x 10^-1 BTU/lb-°F | ||
Thermal Conductivity | 816 BTU-in/hr-ft^2-°F | 816 BTU-in/hr-ft^2-°F | ||
Electrical Conductivity | 29% IACS | 29% IACS |
Chemistry Information
|
|
Element |
Percentage |
Al | 92.4 - 95.6 |
Fe | 0.4 max |
Cr | 0.05 - 0.25 |
Cu | 0.1 max |
Mg | 4 - 4.9 |
Mn | 0.4 - 1 |
Ti | 0.15 max |
Si | 0.4 max |
Residual | 0.15 max |
Zn | 0.25 max |