314, also known as leaded commercial bronze, is a free-machining brass that has superior thermal and electrical conductivity to other alloys of brass, this alloy offers good strength and corrosion resistance as well. The lower zinc content of 314 brass gives it a reddish color along with better resistance to cracking, as well. It is typically used in hardware, electrical components, fasteners, screws, and other industrial applications.
UNS C31400, CDA 314, C314, ISO CuZn9Pb2, Leaded Commercial Bronze
Safety Data Sheet | Weight Calculator | Mill Test Reports
ASTM |
---|
B140 |
Physical Properties 314 | |||||
-H02 | |||||
---|---|---|---|---|---|
Density | 0.319 lb/in3 | ||||
Ultimate Tensile Strength | 52.2 ksi | ||||
Yield Tensile Strength | 45 ksi | ||||
Shear Strength | 29.7 ksi | ||||
Shear Modulus | 6,530 ksi | ||||
Hardness Rockwell | Brinell | B58-61 | 92-96 | ||||
Elongation at Break Percentage | 18% | ||||
Modulus of Elasticity | 16,700 ksi | ||||
Poisson's Ratio | 0.28 | ||||
Machinability Percentage | 80% | ||||
Melting Point | 1,850-1,900 °F | ||||
Specific Heat | 8.96 x 10^-2 BTU/lb-°F | ||||
Thermal Conductivity | 1,250 BTU-in/hr-ft^2-°F | ||||
Electrical Conductivity | 42% IACS |
Chemistry Information
|
|
Element |
Percentage |
Pb | 1.3 - 2.5 |
Zn | 5.8 - 11.2 |
Ni | 0 - 0.7 |
Cu | 87.5 - 90.5 |
Residual | 0 - 0.4 |
Fe | 0 - 0.1 |