Also called Tellurium copper, c145 copper has similar mechanical properties to unalloyed, pure copper but with significantly higher machinability. C145 also maintains good corrosion resistance and excellent electrical conductivity. For hot and cold working, c145 is rated as good, and it can be easily brazed or soldered. Oxyacetylene welding, gas shielded arc welding, and butt welding are just rated at fair. Typically used in high-speed automatic screw machines as well as electrical applications like circuit breaker terminals, hot forged, studs and transformers.
UNS C14500, CDA 145, C145, ISO CuTeP, Tellurium-Bearing Copper
Safety Data Sheet | Weight Calculator | Mill Test Reports
Physical Properties 145 | |||||
-H02 | -H04 | ||||
---|---|---|---|---|---|
Density | 0.323 lb/in3 | 0.323 lb/in3 | |||
Ultimate Tensile Strength | 42.8 ksi | 47 ksi | |||
Yield Tensile Strength | 39.9 ksi | 38 ksi | |||
Shear Modulus | 6,380 ksi | 6,380 ksi | |||
Shear Strength | 26.1 ksi | 27 ksi | |||
Hardness Rockwell | Brinell | B43 | 77 | B48 | 81 | |||
Elongation at Break Percentage | 18% | 12% | |||
Modulus of Elasticity | 16,700 ksi | 16,700 ksi | |||
Poisson's Ratio | 0.31 | 0.31 | |||
Machinability Percentage | 85% | 85% | |||
Melting Point | 1,924-1,967 °F | 1,924-1,967 °F | |||
Specific Heat | 9.2 x 10^-2 BTU/lb-°F | 9.2 x 10^-2 BTU/lb-°F | |||
Thermal Conductivity | 2460 BTU-in/hr-ft^2-°F | 2460 BTU-in/hr-ft^2-°F | |||
Electrical Conductivity | 94% IACS | 94% IACS |
Chemistry Information
|
|
Element |
Percentage |
Cu | 99.5 |
P | 0.008 |
Te | 0.5 |