Product Details, Specifications, and Technical Information
See Stainless Steel Tolerances
Stainless Sheet/Plate 347 provides high strength, high temperature capability, and corrosion resistance in strongly oxidizing environments. 347 is an austenitic stainless and also can operate at high temperatures without losing strength. It is typically used in aerospace for aircraft exhausts, collector rings, expansion joints, and in high temperature chemical processing.
![shape Image](/medias/shape-sheet-sheet-large-new-min-4.png?context=bWFzdGVyfGltYWdlc3w2MjQzfGltYWdlL3BuZ3xhVzFoWjJWekwyaGxPUzlvTlRjdk9EazVPVGt5TlRZM09ERXhNQzV3Ym1jfGUyMTA0MTViNDE5YzYyYjdmMWQ3MTJkZWYzNDRkMGJiMDIxNjA1ZTdkMTk2OGVmMmZmZjZlYThiNTRkOGQ0YWI)
Dimension Name | Specification |
Thickness | 0.125 |
Max Width | 48 |
Max Length | 120 |
Alloy | 347 |
Eniteo Vendor ID | 3143 |
MTR Availability | Yes |
Full Length | true |
Material | Stainless Steel |
Shape | Sheet/Plate |
Custom Cut Warehouse | 1 |
This material meets the following specs: ASTM -A262, ASTM -A240, AMS -5512
Weight/Lineal Foot | ||
5.17 pounds |
Mechanical Properties | |
Property | Value |
Yield Tensile Strength KSI | 39 |
Ultimate Tensile Strength KSI | 93 |
Rockwell Hardness B Scale | 85 |
Density g/cm^3 | 8 |
Shear Strength KSI | 65 |
Brinell Hardness 500 kg load | 167 |
Melting Point °F | 2550 - 2600 |
Machinability % | 36 |
Elongation % in 2 in. | 45 |
Electrical Conductivity % IACS | 2 |
Chemistry Information: 347 Stainless Steel | |
Element | Percentage |
Mn | 2 max |
C | 0.08 max |
P | 0.045 max |
S | 0.03 max |
Si | 0.75 max |
Cr | 17 - 19 |
Ni | 9 - 13 |
Nb + Ta | 1 max |